性能項(xiàng)目 | 測(cè)試條件 | 測(cè)試方法 | 數(shù)值/描述 | 單位 | |
機(jī)械性能 | 拉伸強(qiáng)度(引張強(qiáng)度) | ASTM D638/ISO 527 | 165 | kg/cm2(MPa)[Lb/in2] | |
斷裂伸長(zhǎng)率 | ASTM D638/ISO 527 | % | |||
拉伸模量 | ASTM D638/ISO 527 | kg/cm2(MPa)[Lb/in2] | |||
拉伸屈服伸長(zhǎng)率(延伸率) | ASTM D638/ISO 527 | 1.4 | % | ||
拉伸斷裂伸長(zhǎng)率(延伸率) | ASTM D638/ISO 527 | % | |||
彎曲模量(彎曲彈性率) | ASTM D790/ISO 178 | kg/cm2(MPa)[Lb/in2] | |||
彎曲強(qiáng)度 | ASTM D790/ISO 178 | 250 | kg/cm2(MPa)[Lb/in2] | ||
洛氏硬度 | ASTM D785 | R-123 | |||
IZOD 缺口沖擊強(qiáng)度 | 1/4" 23℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | ||
1/4" -30℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
1/8" 23℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
1/8" -30℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
Charpy沖擊強(qiáng)度 | 23℃ (缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | ||
-30℃(缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
23℃(無(wú)缺口) | ASTM D256/ISO 179 | 30 | kg·cm/cm(J/M)ft·lb/in | ||
-30℃(無(wú)缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
物性性能 | 比重(密度) | ASTM D792/ISO 1183 | 1660 | ||
成型收縮率 | ASTM D955 | % | |||
熔融指數(shù)(流動(dòng)系數(shù)) | 200℃/5kg | ASTM D1238/ISO 1133 | g/10min | ||
220℃/10kg | ASTM D1238/ISO 1133 | g/10min | |||
吸水率 23℃/24H | ASTM D570/ISO 62 | 0.02 | % | ||
熱性能 | 熱變形溫度 | 退火 | ASTM D648/ISO 75 | >260 | ℃(℉) |
未退火 | ASTM D648/ISO 75 | ℃(℉) | |||
維卡軟化點(diǎn) | ASTM D1525/ISO R306 | ℃(℉) | |||
熔點(diǎn) | - | ℃(℉) | |||
燃燒性(率) | UL94 | V-0 (0.28mmt) | |||
線性膨脹系數(shù) | ASTM D696/ISO 11359 | mm/mm.℃ | |||
電氣性能 | 介電常數(shù) | 100HZ | ASTM D150/IEC 60250 | 3.6 | |
1MHZ | ASTM D150/IEC 60250 | ||||
體積電阻率 | ASTM D257/IEC 60093 | 10^14 | Ω.cm | ||
表面電阻率 | ASTM D257/IEC 60093 | Ω | |||
耐電弧性 | ISO 14782 | ||||
加工條件 | 干燥條件 | ||||
加工溫度 | 射嘴 | ℃ | |||
料筒前段 | ℃ | ||||
料筒中段 | ℃ | ||||
料筒后段 | ℃ | ||||
熔體溫度 |