Hardness(Shore)硬度:77A
Specific Gravity比重/密度:1.18 g/cm3
Tensile Stress拉伸率 (kgf/cm2)
At elongation 35
At 300% elongation 65
Tensile Strength拉伸強(qiáng)度:300 kgf/cm2
Ultimate Elongation大拉長(zhǎng):800%
Tear Resistance (Die C)抗撕裂性:80 kgf/cm
Abrasion Loss磨損量:40 mm3 loss
Compression Set壓縮率
At 23°C X22hr 15 %
At 70°C X22hr 30%
Vicat Softening Temperature維卡溫度:84°C
S180A
Hardness(Shore)硬度:83A
Specific Gravity比重/密度:1.19 g/cm3
Tensile Stress拉伸率 (kgf/cm2)
At elongation 45
At 300% elongation 90
Tensile Strength拉伸強(qiáng)度:350 kgf/cm2
Ultimate Elongation大拉長(zhǎng):770%
Tear Resistance (Die C)抗撕裂性:90 kgf/cm
Abrasion Loss磨損量:30 mm3 loss
S185A
Hardness(Shore)硬度:87A
Specific Gravity比重/密度:1.2g/cm3
Tensile Stress拉伸率 (kgf/cm2)
At elongation 65
At 300% elongation 120
Tensile Strength拉伸強(qiáng)度:400kgf/cm2
Ultimate Elongation大拉長(zhǎng):650%
Tear Resistance (Die C)抗撕裂性:110 kgf/cm2
Abrasion Loss磨損量:30 mm3 loss
Compression Set壓縮率
At 23°C X22hr 15 %
At 70°C X22hr 35%
Vicat Softening Temperature維卡溫度:95°C有意者請(qǐng)致電陳先生:13145830621,謝謝!